Product details
Greenlogy TEC
Pultruded FRP grating is made with pultruded "I"-shaped and "T"-shaped profiles as load-bearing bars and solid tubes or rods as connecting rods, assembled through a certain assembly process into grating with gaps left in the panel surface.
Name | Contact Information | Type |
|---|---|---|
Resin | 25% | OFR-25,IFR-25,VEFR-25 |
Glass Fiber | 65% | E |
Filler | 8% | ATH,PR |
Other | 2% | --- |
Code | Resin Type | Flame Retardancy | Recommended Applications |
|---|---|---|---|
MP-5 | Phenolic Type | Oxygen index can reach about 80 | Low toxicity, high flame retardancy, suitable for applications with high fire-safety requirements |
VEFR-25 | Vinyl Ester Type | Oxygen index 28 and above | Harsh environments with strong acid, alkali and other corrosive media |
VEFR-10 | Vinyl Ester Type | Oxygen index 35 and above | Strong acids, strong alkalis and other demanding applications where higher flame retardancy is required |
IFR-25 | Isophthalic Type | Oxygen index 28 and above | VEFR economical type, good performance, resistant to moderate acids, alkalis and solvents |
IFGR-30 | Benzene-based, food grade | Oxygen index 26 | Mainly used in meat products and food processing plants |
OFR-25 | Orthophthalic type | Oxygen index 28 and above | General acid and alkali environments |
OCR | Orthophthalic type | Oxygen index below 28 | OFR-25 economical type, no flame retardancy requirement |
Coarse glass fiber type selection
Code | Coarse grit type | Recommended Applications |
E | Alkali-free glass grit | For applications requiring high strength and high corrosion resistance |
Filler type selection
Code | Filler type | Recommended Applications |
|---|---|---|
ATH | Aluminum hydroxide | Flame-retardant, smoke-suppressing and corrosion-resistant applications |
PR | No filler, pure resin | For highly corrosion-resistant applications |
Standard panel size:
Width 1220mm, 915mm; length 3050mm, 6100mm
Bearing bar: 25mm
Open area: 33%
Approx. weight (incl. three cores): 11.2kg/m²
Line load (unit: mm)
Spacing | kg/m | kg/m | kg/m | kg/m | kg/m | kg/m | Limit |
|---|---|---|---|---|---|---|---|
(mm) | 300 | 450 | 750 | 1500 | 3000 | 5950 | Load |
| 450 | 0.58 | 0.86 | 1.45 | 2.87 | 5.74 | --- | 10309 |
| 600 | 1.27 | 1.93 | 3.23 | 6.45 | --- | --- | 7731 |
| 900 | 4.01 | 5.99 | 10.1 | --- | --- | --- | 5024 |
| 1200 | 8.99 | --- | --- | --- | --- | --- | 3620 |
Uniformly distributed load (unit: mm)
Spacing | kg/m² | kg/m² | kg/m² | kg/m² | kg/m² | kg/m² | Limit |
|---|---|---|---|---|---|---|---|
(mm) | 1000 | 1900 | 3900 | 7000 | 9500 | 19500 | Load |
| 450 | 0.56 | 1.07 | 2.13 | 4.04 | 5.23 | --- | 45076 |
| 600 | 1.63 | 3.23 | 6.54 | 12.1 | --- | --- | 25363 |
| 900 | 7.52 | 15 | --- | --- | --- | --- | 10971 |
| 1200 | --- | --- | --- | --- | --- | --- | 5938 |
Features:
Flame retardant
Highly flame retardant
Low smoke, non-toxic gas release
High strength-to-weight ratio
Corrosion resistant
Low maintenance
Anti-slip
Non-conductive and thermally insulating
Easy to fabricate
Impact resistance
UV resistance
Maintenance-free
Installation and accessories
Applications
Pultruded Grating T-3310 is suitable for platforms, walkways, trench covers, stair treads and equipment operating surfaces that require a combination of load-bearing capacity, corrosion resistance, and ventilation and drainage. It is commonly used in chemical, water treatment, electroplating, marine engineering and power applications involving damp, acid-base or salt-spray environments. If your operating conditions involve high temperatures, severe corrosion or special loads, please contact us to confirm a suitable solution based on the specific medium, span and installation method.
Selection guide
When selecting, we recommend first clarifying the resin system (such as OFR, IFR, VEFR or phenolic types, corresponding to different flame-retardant and corrosion-resistance orientations), the load-bearing direction and the support span, then confirming the grating thickness, mesh spacing and connection method to match the actual load and installation conditions. Because different resin and fiber ratios affect strength, flame retardancy and corrosion resistance, please contact us with your operating parameters and we will assist with selection and specification confirmation. For detailed specifications and quotations, please contact us.
Product advantages
Pultruded Grating T-3310 uses pultruded "I"-shaped and "T"-shaped profiles as load-bearing bars, combined with solid tubes or rods as connecting rods, assembled according to a certain process with gaps left in the panel surface, so it combines relatively high longitudinal load-bearing capacity with light weight, corrosion resistance and ease of cutting and installation. This structure facilitates ventilation, drainage and light transmission, and is non-conductive and non-magnetic, making it suitable as a replacement for some metal gratings in corrosive environments. Specific performance varies with resin and fiber configuration; please contact us to confirm the applicable configuration.
Inquiry prompt
For further information on the detailed specifications, resin selection recommendations and commercial terms of Pultruded Grating T-3310, please contact us and provide your operating environment, load requirements and dimensional needs; we will provide a targeted solution and quotation accordingly. Please contact us for detailed specifications and quotations.