Product details
Greenlogy TEC
Pultruded FRP grating is a panel with gaps made through a defined assembly process, using pultruded "I"-shaped and "T"-shaped profiles as bearing bars and solid tubes or rods as connecting rods.
Name | Content | Type |
|---|---|---|
Resin | 25% | OFR-25,IFR-25,VEFR-25 |
Glass fiber | 65% | E |
Filler | 8% | ATH,PR |
Other | 2% | --- |
Code | Resin type | Flame retardant performance | Recommended application |
|---|---|---|---|
MP-5 | Phenolic type | Oxygen index can reach about 80 | Low toxicity and high flame retardancy, for applications where fire safety requirements are critical |
VEFR-25 | Vinyl type | Oxygen index 28 and above | Harsh corrosive environments such as acid and alkali |
VEFR-10 | Vinyl type | Oxygen index 35 and above | Strong acid and strong alkali with high flame retardant requirements and favorable service environments |
IFR-25 | Isophthalic type | Oxygen index 28 and above | VEFR economical type, good performance, resistant to moderate acids, alkalis and solvents |
IFGR-30 | phthalic food grade | oxygen index 26 | mainly used for meat products and food processing plants |
OFR-25 | orthophthalic type | Oxygen index 28 and above | general acid and alkali environments |
OCR | orthophthalic type | oxygen index below 28 | OFR-25 economical type, no flame retardancy requirement |
coarse glass fiber selection
Code | coarse sand type | Recommended application |
E | E-glass sand | for high-strength requirements and highly corrosion-resistant applications |
filler type selection
Code | filler type | Recommended application |
|---|---|---|
ATH | aluminum hydroxide | flame-retardant, smoke-suppressing and corrosion-resistant applications |
PR | no filler, pure resin | for highly corrosion-resistant applications |
Standard panel size:
1220mm, 915mm wide; 3050mm, 6100mm long
Bearing bar: 38mm
Open area: 25%
Approximate weight (including three-strand wire): 16.7kg/m²
Pad load (unit: mm)
Spacing | kg/m | kg/m | kg/m | kg/m | kg/m | kg/m | Limit value |
|---|---|---|---|---|---|---|---|
(mm) | 150 | 300 | 450 | 750 | 1500 | 3000 | Load |
| 450 | <0.25 | 0.25 | 0.25 | 0.51 | 1.02 | 2.29 | 7539 |
| 600 | 0.25 | 0.51 | 0.51 | 1.02 | 2.03 | 4.06 | 6020 |
| 900 | 0.51 | 1.27 | 1.78 | 3.05 | 6.35 | 12.4 | 4023 |
| 1200 | 1.52 | 2.79 | 4.32 | 7.11 | --- | --- | 3010 |
Uniformly distributed load (unit: mm)
Spacing | kg/m² | kg/m² | kg/m² | kg/m² | kg/m² | kg/m² | Limit value |
|---|---|---|---|---|---|---|---|
(mm) | 450 | 950 | 1450 | 2400 | 4850 | 9500 | Load |
| 450 | <0.25 | 0.25 | 0.25 | 0.51 | 1.02 | 2.03 | 16494 |
| 600 | 0.25 | 0.51 | 0.76 | 1.27 | 2.54 | 5.08 | 12346 |
| 900 | 1.27 | 2.29 | 3.56 | 5.84 | 11.7 | --- | 8247 |
| 1200 | 3.56 | 7.11 | 10.7 | --- | --- | --- | 4929 |
Features:
Flame retardant
High flame retardancy
Low smoke and low-toxicity emissions
High strength-to-weight ratio
Corrosion resistant
Low maintenance
Anti-slip
Electrical and thermal insulation
Easy to process
Impact resistance
UV resistance
Maintenance-free
Installation and accessories
Application scenarios
Pultruded grating T-2515 is assembled from pultruded I/T load-bearing bars with solid tubes or rods as connecting rods, suitable for platforms, walkways, trench covers and various industrial operating surfaces that require load bearing, corrosion resistance and drainage and air flow. For load and span requirements in specific scenarios, please contact us to confirm the selection based on your operating conditions.
Selection guide
When selecting, match the resin system (such as orthophthalic, isophthalic, vinyl ester or phenolic, etc.), load-bearing bar specifications and grating spacing to the service environment and load requirements; for highly corrosive or high fire-safety applications, the corresponding resin type can be given priority. Please provide the service environment, span and load conditions, and we will assist you in determining the appropriate configuration.
Product advantages
Pultruded grating uses continuous pultruded profiles as load-bearing units, with fibers continuously distributed along the load direction, combining relatively high longitudinal strength, light weight and corrosion resistance, and the assembled structure facilitates cutting and on-site installation. The surface can be treated for slip resistance, making it suitable for wet or slippery environments.
Inquiry guide
For detailed specifications, resin and color options, supply forms and commercial terms of pultruded grating T-2515, please contact us for detailed specifications and a quotation. Please let us know your application scenario and quantity requirements, and we will respond promptly with selection advice and a proposal.
Service environment
- Suitable for outdoor walkways, platforms and stair treads; its pultruded FRP load-bearing bars and rod connectors resist outdoor weathering without rusting.
- Suitable for indoor factory environments that are damp or high in humidity, because glass fiber reinforced profiles do not corrode under wet conditions like steel.
- Recommended for chemically corrosive environments such as industrial floors and process areas, where its resin-rich pultruded surface resists splashes and fumes better than metal grating.