Greenlogy TEC
Pultruded FRP grating is manufactured using pultruded "I"-shaped and "T"-shaped profiles as load-bearing bars and solid tubes or rods as connecting rods, assembled through a defined assembly process, with open gaps left in the grating surface.
Name | Content | Type |
|---|---|---|
Resin | 25% | OFR-25,IFR-25,VEFR-25 |
Glass fiber | 65% | E |
Filler | 8% | ATH,PR |
Other | 2% | --- |
Code | Resin type | Flame retardant performance | Recommended application |
|---|---|---|---|
MP-5 | Phenolic type | Oxygen index up to about 80 | Low toxicity and high flame retardancy; for applications where fire safety requirements are critical |
VEFR-25 | Vinyl type | Oxygen index 28 and above | Harsh corrosive environments such as acid and alkali |
VEFR-10 | Vinyl type | Oxygen index above 35 | Acid and alkali environments with high flame-retardant requirements, and favorable environments |
IFR-25 | Isophthalic type | Oxygen index 28 and above | VEFR type: economical, with good performance, resistant to moderate acids, alkalis and solvents |
IFGR-30 | Benzene-based, food grade | Oxygen index 26 | Mainly used in meat processing and food processing plants |
OFR-25 | Orthophthalic type | Oxygen index 28 and above | General acid and alkali environments |
OCR | Orthophthalic type | Oxygen index below 28 | OFR-25 economical type, no flame retardancy requirement |
Coarse glass fiber selection
Code | Coarse sand type | Recommended application |
E | Alkali-free sand | For applications requiring high strength and high corrosion resistance |
Filler selection
Code | Filler type | Recommended application |
|---|---|---|
ATH | Aluminum hydroxide | Flame-retardant, smoke-suppressing and corrosion-resistant applications |
PR | No filler, pure resin | For high corrosion resistance applications |
Standard panel sizes:
Width 1220 mm, 915 mm; length 3050 mm, 6100 mm
Load-bearing flat bar: 50 mm
Open area: 60%
Approximate weight (including three-strand hemp core): 20.1 kg/m²
Line load (unit: mm)
Spacing | kg/m | kg/m | kg/m | kg/m | kg/m | kg/m | kg/m |
|---|---|---|---|---|---|---|---|
(mm) | 300 | 750 | 1000 | 1500 | 2000 | 2500 | 3000 |
| 450 | 0.09 | 0.23 | 0.3 | 0.46 | 0.61 | 0.76 | 0.92 |
| 600 | 0.21 | 0.54 | 0.72 | 1.09 | 1.45 | 1.82 | 2.18 |
| 900 | 0.73 | 1.84 | 2.46 | 3.69 | 4.92 | 6.15 | 7.38 |
| 1200 | 1.75 | 4.37 | 5.83 | 8.75 | 11.7 | 14.5 | --- |
Uniform load (unit: mm)
Spacing | kg/m² | kg/m² | kg/m² | kg/m² | kg/m² | kg/m² | kg/m² |
|---|---|---|---|---|---|---|---|
(mm) | 1000 | 2000 | 3000 | 4000 | 5000 | 7000 | 8000 |
| 450 | 0.19 | 0.38 | 0.57 | 0.76 | 0.96 | 1.34 | 1.53 |
| 600 | 0.45 | 0.91 | 1.36 | 1.82 | 2.27 | 3.19 | 3.64 |
| 900 | 1.53 | 3.07 | 4.61 | 6.15 | 7.69 | 10.7 | 12.4 |
| 1200 | 3.64 | 7.29 | 11 | 14.6 | --- | --- | --- |
Features:
Flame retardant
High fire resistance
Low smoke and low-toxicity emissions
High strength-to-weight ratio
Corrosion resistant
Low maintenance
Anti-slip
Non-conductive and non-heat-conductive
Easy to process
Impact resistant
UV resistant
Maintenance-free
Installation and accessories
Application Scenarios
Pultruded grating I-6020 is commonly used in industrial platforms, walkways, trench covers and chemical, wastewater treatment, marine engineering and other environments that require load-bearing, corrosion-resistant and ventilated grating. The load capacity, span and installation method for specific scenarios must be confirmed based on working conditions; please contact us to discuss selection.
Selection Guide
When selecting, focus on the resin system, grating height, bearing bar spacing and connecting rod type to match the corrosion resistance level, fire protection requirements and load conditions. We can provide recommended solutions based on your operating environment and installation dimensions; please contact us for detailed specifications and quotations.
Product Advantages
Assembled from pultruded I-shaped bearing bars and connecting rods, it features light weight, high strength, corrosion resistance, non-conductivity and easy cutting and installation, making it suitable for replacing some metal gratings. Different resin types have different emphases on flame retardancy and chemical resistance, and can be selected as needed.
Inquiry Guide
To learn about the specifications, supply cycle and commercial terms of pultruded grating I-6020, please provide information such as the operating environment, dimensions and quantity; please contact us for detailed specifications and quotations.
Operating Environment
- Pultruded FRP I-6020 grating is made of pultruded I-shaped profiles with high glass fiber content and a resin matrix, and is suitable for indoor and outdoor installation environments where moisture is present.
- The phenolic MP-5 resin option offers low toxicity and high flame retardancy, with a limiting oxygen index of approximately 80, making it suitable for enclosed industrial areas with fire safety requirements.
- Optional vinyl ester (VEFR-25) and other resin systems make the grating corrosion-resistant in common acid, alkali and salt environments such as chemical processing, wastewater treatment and marine applications.
- It can be used in wet, condensing or washdown conditions; for high-temperature or high-concentration chemical contact applications, please contact us for the complete parameter table and resin selection guidance.