Product details
Greenlogy TEC
Pultruded FRP grating is made of pultruded "I", "T" shaped profile as a bearing strip, with a solid pipe or bar as a connecting rod, made by a certain assembly process with a gap of the plate.
Name | Contect | Type |
|---|---|---|
Resin | 25% | OFR-25,IFR-25,VEFR-25 |
Fiberglass | 65% | E |
Filler | 8% | ATH,PR |
Others | 2% | --- |
Code | Resin type | Flame retardant property | Recommended usage occasions |
|---|---|---|---|
MP-5 | Phenolic type | Oxygen index can reach about 80 | Low toxicity and high flame retardant, fire safety is very important for the occasion |
VEFR-25 | Vinyl type | Oxygen index 28 or above | Acid, alkali and other corrosive harsh environment |
VEFR-10 | Vinyl type | Oxygen index 35 or above | Flame retardant requirements of high acid, alkali and good occasions |
IFR-25 | Meta benzene | Oxygen index 28 or above | A VEFR type economy, and excellent, moderate acid alkali and solvent |
IFGR-30 | Benzene food grade | Oxygen index 26 | Mainly used in meat products and food processing plants |
OFR-25 | Ortho type | Oxygen index 28 or above | General acid and alkali environment |
OCR | Ortho type | Oxygen index below 28 | OFR-25 economy, no flame retardant requirements |
The type selection of coarse glass fiber
Code | Coarse sand type | Recommended usage occasions |
E | Non alkali sand | For high strength requirements and high corrosion resistance of the occasion |
Selected filler type
Code | Filler type | Recommended usage occasions |
|---|---|---|
ATH | Aluminum hydroxide | Retardant, smoke suppression, corrosion-resistant occasions |
PR | No filler, pure resin | For high corrosion-resistant applications |
Standard Panel Size:
1220mm,915mm-wide 3050mm,6100mm-length
Bearing Bar: 32mm
Open Area: 50%
Approx Weight (With three-core shoots): 17.4kg/m²
The characteristics:
Fire Retardant
High Flame Resistance
Low Smoke and Toxic Fume Emissions
High Strength-to-Weight Ratio
Corrosion Resistant
Low Maintenance
Slip Resistant
Electrically & Thermally Non-Conductive
Easily Fabricated
Impact Resistant
UV resistance
Maintenance free
Installation and accessories
Application Scenarios
Pultruded Grating I-50125 is suitable for platforms, walkways, trench covers and equipment operating surfaces that require both load-bearing capacity and corrosion resistance. It is commonly used in humid or corrosive environments such as chemical, wastewater treatment, marine engineering and power industries. Suitability for specific scenarios must be confirmed based on span, load and media conditions.
Selection Guide
When selecting, please focus on the load-bearing direction, support span, service load and corrosive media type, so as to determine the resin system, load-bearing bar specifications and connecting rod spacing. You are welcome to contact us with your operating parameters, and we will assist in recommending a suitable grating configuration and resin type.
Product Advantages
Assembled from pultruded I-shaped load-bearing bars and solid tube/rod connecting rods, it has strong structural directionality and a high strength-to-weight ratio in the load-bearing direction. The FRP material itself is corrosion-resistant, non-conductive and non-magnetic, making it easy to cut and install on site and suitable as an alternative to traditional metal grating.
Inquiry Guide
For detailed specifications, resin options and supply information for I-50125, please contact us. We will provide quotations and technical support based on your project requirements.
Operating Environment
- This pultruded FRP grating is built for both indoor and outdoor installations, where its pultruded I-shaped bearing bars and pipe or bar connecting rods resist moisture and weathering without the corrosion problems of steel grating.
- It is suited to humid and wet service areas such as walkways, platforms, stair treads and trench covers in plants where condensation, washdown or splash is present.
- The grating tolerates exposure to mildly corrosive media; for strongly acidic or alkaline environments, select the resin type (for example VEFR-25 vinyl type with an oxygen index of 28 or above, as listed in the resin introduction above) and confirm suitability with us before ordering.
- For installations exposed to elevated temperatures, fire-risk zones or low-toxicity and high flame-retardant requirements, the MP-5 phenolic type resin with an oxygen index of about 80 is the recommended option; contact us to discuss the operating temperature range and resin choice for your site.