  Pultruded FRP grating is made with pultruded "I"-type and "T"-type profiles as load-bearing bars and solid tubes or rods as connecting rods, fabricated through a specific assembly process, with gaps left in the panel surface.  

Name

Content

Type

Resin

25%

OFR-25,IFR-25,VEFR-25

Glass fiber

65%

E

Filler

8%

ATH,PR

Other

2%

---

Raw material introduction
Resin type

Code

Resin type

Flame retardant performance

Recommended applications

MP-5

Phenolic type

Limiting oxygen index up to about 80

Low toxicity and high flame retardancy, for applications with high fire safety requirements

VEFR-25

Vinyl ester type

Limiting oxygen index 28 and above

Harsh corrosive environments such as acids and alkalis

VEFR-10

Vinyl ester type

Limiting oxygen index 35 and above

Acid and alkali environments requiring high flame retardancy and good performance

IFR-25

Isophthalic polyester type

Limiting oxygen index 28 and above

VEFR economical type, good performance, resistant to moderate acids, alkalis and solvents

IFGR-30

Styrene-based, food grade

Oxygen index 26

Mainly used for meat products and food processing plants

OFR-25

Orthophthalic type

Limiting oxygen index 28 and above

General acid and alkali environments

OCR

Orthophthalic type

Oxygen index below 28

OFR-25 economical type, no flame retardancy requirement

Coarse glass fiber selection   

Code

Coarse grit type

Recommended applications

E

Alkali-free (E-glass) grit

For high-strength requirements and highly corrosion-resistant applications

Filler type selection  

Code

Filler type

Recommended applications

ATH

Aluminum hydroxide

Flame-retardant, smoke-suppressing and corrosion-resistant applications

PR

No filler, pure resin

For highly corrosion-resistant applications

Sand surface

Smooth surface

Anti-slip grooved surface

Standard panel sizes:
Width 1220 mm, 915 mm; length 3050 mm, 6100 mm
Load-bearing flat bar: 38 mm
Open area: 40%

Approx. weight (incl. three-core strand): 22 kg/m²

Line load (unit: mm)

Spacing

kg/m

kg/m

kg/m

kg/m

kg/m

kg/m

Limit value

(mm)

300450750150030005950

Load

4500.120.250.510.761.522.7926215
6000.290.511.021.783.055.8419661
9001.021.272.295.329.3817.812705
12002.953.595.579.419.138.99086

Uniform load (unit: mm)

Spacing

kg/m²

kg/m²

kg/m²

kg/m²

kg/m²

kg/m²

Limit value

(mm)

1000190039007000950019500

Load

4500.250.450.761.672.424.83114645
6000.611.182.324.595.969.6264506
9001.923.796.3311.215.5---27757
12004.969.64------------14905

Features:

  • Flame retardant

  • High flame retardancy

  • Low smoke and low toxicity emissions

  • High strength-to-weight ratio

  • Corrosion resistant

  • Low maintenance

  • Anti-slip

  • Electrical and thermal insulation (non-conductive)

  • Easy to process

  • Impact resistance 

  • UV resistance

  • Maintenance-free

Installation and accessories


Applications

Pultruded Grating I-4015 is assembled with pultruded "I"-shaped load-bearing bars and solid tubes or rods as connecting rods, suitable for platforms, walkways, trench covers and various industrial operating surfaces that require load-bearing capacity and corrosion resistance. In chemical, water treatment, electroplating, marine and general corrosive media environments, different resin systems can be selected according to specific working conditions. Please contact us to describe your operating environment so we can confirm a suitable solution.

Selection guide

When selecting, it is recommended to first clarify the medium type and concentration, ambient temperature, load type and installation support span, and then choose the resin type (such as phenolic type, vinyl type, etc.) as well as grating thickness and load-bearing bar spacing accordingly. Different resins have different emphases in flame retardancy and corrosion resistance. Please contact us for specific specifications and load data.

Product advantages

Pultruded grating uses continuous pultruded profiles as load-bearing units and features light weight, high strength, corrosion resistance, non-conductivity and maintenance-free performance. It is easy to cut and install on site and can reduce later maintenance costs. Its surface can be made slip-resistant to improve walking safety. For detailed performance information, please contact us.

Inquiry guidance

If you would like to know the detailed specifications, resin options, load-bearing capacity and quotation of Pultruded Grating I-4015, please contact us and provide your operating conditions and dimension requirements. We will recommend a suitable solution and provide a quotation.