Pultruded FRP grating is made by using pultruded "I"-shaped and "T"-shaped profiles as load-bearing bars and solid tubes or rods as connecting rods, assembled through a specific assembly process, with gaps left between the panel joints.
Name | Content | Type |
|---|---|---|
Resin | 25% | OFR-25,IFR-25,VEFR-25 |
Glass fiber | 65% | E |
Filler | 8% | ATH,PR |
Other | 2% | --- |
Code | Resin type | Flame retardancy | Recommended applications |
|---|---|---|---|
MP-5 | Phenolic type | Oxygen index up to about 80 | Low toxicity and high flame retardancy; applications with very high fire safety requirements |
VEFR-25 | Vinyl ester type | Oxygen index 28 and above | Harsh environments with strong acid and alkali corrosion |
VEFR-10 | Vinyl ester type | Oxygen index 35 and above | Applications requiring high flame retardancy and resistance to strong acid and alkali corrosion |
IFR-25 | Isophthalic resin | Oxygen index 28 and above | VEFR economical type, good performance, resistant to moderate acids, alkalis and solvents |
IFGR-30 | Styrene-based (benzene-type) resin, food grade | Oxygen index 26 | Mainly used for meat products and food processing plants |
OFR-25 | Orthophthalic type | Oxygen index 28 and above | General acid and alkali environments |
OCR | Orthophthalic type | Oxygen index below 28 | OFR-25 economical type, no flame-retardant requirement |
Coarse glass fiber type selection
Code | Coarse glass fiber type | Recommended applications |
E | Alkali-free glass (E-glass) | For applications requiring high strength and high corrosion resistance |
Selected filler type
Code | Filler type | Recommended applications |
|---|---|---|
ATH | Aluminum hydroxide | Flame-retardant, smoke-suppressing and corrosion-resistant applications |
PR | No filler, pure resin | For high corrosion resistance applications |
Standard panel size:
1220mm, 915mm wide; 3050mm, 6100mm long
Load-bearing bar: 50mm
Open area: 60%
Approx. weight (incl. three-core strand): 43.5kg/m²
Line load (unit: mm)
Spacing | kg/m | kg/m | kg/m | kg/m | kg/m | kg/m | kg/m | kg/m | kg/m |
|---|---|---|---|---|---|---|---|---|---|
(mm) | 150 | 300 | 450 | 750 | 1500 | 3000 | 4500 | 6000 | 7500 |
| 600 | 0.05 | 0.1 | 0.13 | 0.23 | 0.46 | 0.89 | 1.35 | 1.78 | 2.24 |
| 750 | 0.08 | 0.15 | 0.25 | 0.4 | 0.81 | 1.63 | 2.44 | 3.28 | 4.09 |
| 900 | 0.13 | 0.28 | 0.41 | 0.69 | 1.37 | 2.74 | 4.09 | 5.46 | 6.83 |
| 1200 | 0.33 | 0.64 | 0.97 | 1.6 | 3.2 | 6.4 | 9.6 | 12.8 | 16 |
Uniform load (unit: mm)
Spacing | kg/m² | kg/m² | kg/m² | kg/m² | kg/m² | kg/m² | kg/m² | kg/m² | kg/m² |
|---|---|---|---|---|---|---|---|---|---|
(mm) | 450 | 950 | 1450 | 2450 | 4850 | 9800 | 14500 | 19500 | 24400 |
| 600 | 0.05 | 0.1 | 0.18 | 0.28 | 0.56 | 1.12 | 1.68 | 2.24 | 2.77 |
| 750 | 0.13 | 0.25 | 0.38 | 0.64 | 1.27 | 2.55 | 3.84 | 5.11 | 6.38 |
| 900 | 0.25 | 0.51 | 0.76 | 1.27 | 2.57 | 5.13 | 7.67 | 10.2 | 12.8 |
| 1200 | 0.81 | 1.6 | 2.41 | 4.01 | 8 | 16 | --- | --- | --- |
Features:
Flame retardant
High fire resistance
Low smoke and low toxicity emissions
High strength-to-weight ratio
Corrosion resistant
Low maintenance
Anti-slip
Non-conductive and non-heat-conductive
Easy to process
Impact resistant
UV resistant
Maintenance-free
Installation & Accessories
Application Scenarios
Pultruded grating is assembled using pultruded "I" and "T" profiles as load-bearing bars and solid tubes or rods as connecting rods. It is suitable for platforms, walkways, trench covers and equipment operating surfaces that require load-bearing capacity, corrosion resistance and flame retardancy. Different resin systems suit different service conditions; for specific selection, please contact us to confirm based on your actual working conditions.
Selection Guide
Selection mainly depends on media corrosiveness, load-bearing requirements and fire protection requirements: phenolic types have a high oxygen index and are suitable for applications with high requirements for low toxicity, high flame retardancy and fire safety; vinyl ester types offer good corrosion resistance and are suitable for common acid and alkali environments. Welcome to contact us for detailed specifications and quotations; we will help match the resin type and grating structure.
Product Advantages
Assembled from pultruded profiles, the panels are lightweight, high-strength, corrosion-resistant and easy to cut and install on site, reducing later maintenance. The open-gap structure between profiles and connecting rods accommodates both load bearing and drainage and ventilation, making it suitable for a variety of industrial environments.
Inquiry Guide
For specific information on the size, resin type, load bearing and delivery time of pultruded grating HL-6020, please contact us. We will provide detailed specifications and quotations based on your working conditions.
Service Environment
- Pultruded FRP grating HL-6020 uses pultruded I-type and T-type load-bearing bars as its framework, connected with solid tubes or solid rods as connecting rods. This structure is suitable for walking surfaces where steel materials would corrode.
- The phenolic MP-5 resin option is formulated for low-toxicity, high-flame-retardancy applications and is suitable for indoor and outdoor locations with fire safety requirements.
- The vinyl ester and other resin systems in the series are selected for service conditions involving long-term exposure to damp, chemical-containing or other corrosive environments.
- Typical application locations include platform walkways, stair treads and inspection covers in industrial plants; please contact us and provide your site conditions to obtain the complete parameter table.