Product Category

Product details

Product Details

The 6x7 construction general-purpose wire rope is available with either FC (imported fiber core) or WSC (wire strand core). When the core is a wire strand core, the rope is usually referred to as 7x7. Wire ropes with diameters from 0.5 mm to 2 mm are common, and the rope is flexible overall. The 6x7 wire rope becomes very stiff at larger diameters, typically beginning to stiffen at 6 mm and above, and is often used for belt conveying, ropeway haulage, fishing operations and similar applications.

Surface treatment: bright or galvanized

Standard: GB/T 20118-2006

Engineering Applications

  • Construction Engineering Applications

  • Small-diameter wire rope slings

  • Guy wires

  • Fencing cables

  • Slings

  • Garage door wire ropes

  • Fixed guy wires

  • Tagline ropes

  • Cable car ropes

Breaking load



Minimum breaking load
Minimum breaking load
DiameterWeight(1770Mpa)
(1770Mpa)
mm
Kg/m
KN
Kg
20.012.35239
30.03
5.29
539
40.06
9.4
959
50.09
14.7
1498
60.13
21.2
2157
70.17
28.8
2937
80.22
37.6
3836
90.27
47.6
4855
100.34
58.8
5993
110.42
71.1
7252
120.51
84.6
8631
140.68
115
11748
160.88
150
15344
181.1
190
19420
201.36
235
23975
221.61
284
29010
241.96
338
34525
262.28
397
40518
282.61
461
46992
302.98
529
53945
323.53
602
61377
364.47
762
77681
405.52
940
95902

General-purpose engineering wire rope

Greenlogy TEC (LM) specializes in supplying multi-strand bright or galvanized wire rope. Our products range in diameter from 0.5 mm to 64 mm and include 1x19, 7x7, 6x19, 7x19, 6x36, 8x19, 8x36, 19x7 and 35x7 specifications with fiber cores and steel cores. In addition to these standard wire ropes, we can also supply premium special wire ropes.

Most wire ropes work under demanding conditions and must have resistance to crushing, bending fatigue and wear. All of our wire ropes are designed for high performance to extend service life and thereby increase end-user productivity. We therefore ensure that all materials are produced in accordance with wire rope industry standards. Every wire rope can be supplied with fittings such as thimbles, swaged terminals and wedge sockets as well as many other assembly components. We also offer customization services; our engineering team can manufacture wire ropes to your required specifications. All materials are certified, traceable and compliant with ISO9001.

Selection Guide

When selecting 6x7 wire rope, factors such as load requirements, flexibility, corrosion resistance and the working environment should be considered comprehensively. For applications requiring higher flexibility, a smaller diameter or fiber core (FC) construction is recommended; if higher strength is required, a wire strand core (WSC) construction can be considered. For specific selection parameters, please contact us for detailed specifications and quotations.

Product Advantages

The 6x7 steel wire rope offers high breaking strength and good flexibility, making it suitable for a wide range of engineering applications. Bright or galvanized surface finishes meet different anti-corrosion requirements. It is produced in strict accordance with GB/T 20118-2006 to ensure reliable quality. For more information on product advantages and suitable applications, please contact us.

Inquiry Guide

For detailed technical parameters, pricing and delivery terms, please contact us through the contact details on our website. Our professional team will provide customized solutions based on your requirements. Please contact us for detailed specifications and quotations.