Name | Content | Type |
|---|---|---|
Resin | 35% | OFR-25,IFR-25,VEFR-25 |
Fiberglass | 33% | E |
Filler | 31% | ATH,PR |
Others | 1% | --- |
Introduction of raw materials
Resin type
Code | Resin type | Flame retardant property | Recommended usage occasions |
|---|---|---|---|
MP-5 | Phenolic type | Oxygen index can reach about 80 | Low toxicity and high flame retardant, fire safety is very important for the occasion |
VEFR-25 | Vinyl type | Oxygen index 28 or above | Acid, alkali and other corrosive harsh environment |
VEFR-10 | Vinyl type | Oxygen index 35 or above | Flame retardant requirements of high acid, alkali and good occasions |
IFR-25 | Meta benzene | Oxygen index 28 or above | A VEFR type economy, and excellent, moderate acid alkali and solvent |
IFGR-30 | Benzene food grade | Oxygen index 26 | Mainly used in meat products and food processing plants |
OFR-25 | Ortho type | Oxygen index 28 or above | General acid and alkali environment |
OCR | Ortho type | Oxygen index below 28 | OFR-25 economy, no flame retardant requirements |
The type selection of coarse glass fiber
Code | Coarse sand type | Recommended usage occasions |
E | Non alkali sand | For high strength requirements and high corrosion resistance of the occasion |
Selected filler type
Code | Filler type | Recommended usage occasions |
|---|---|---|
ATH | Aluminum hydroxide | Retardant, smoke suppression, corrosion-resistant occasions |
PR | No filler, pure resin | For high corrosion-resistant applications |
Feature One
Feature Two
Feature Three
83*83*40(mm)
Panel size available:
1007*4007,1007*3007 Bidirectional force.
Bearing bar thickness (Top/Bottom):7.0/5.0
Bearing bar center:83
Open Aera:84%
Approx Weight:9.5kgs/m²
The characteristics:
Corrosion Resistant
Slip Resistant
Superior Ergonomics
Low Install Cost
Fire Retardant
Lightweight,Bi-directional Strength, and the cutting makes the pipes easier to install.
The internal and external uniform color and color can be arbitrary choice.
It has good social and economic benefits.
Can design , flexible and varied size, size stability
Widely used in:
Greenlogy TEC FRP grating is widely used in landing (industrial) floor, stairs and walkways and platforms. Using glass fiber reinforced plastic grille has many advantages: glass fiber reinforced plastic grille, weather resistance, low maintenance cost, has a long service life and good anti-skid performance. In addition, the glass fiber reinforced plastic grille is simple, fast, flexible processing and assembly.
Application Scenarios
The combination of 83*83 mesh size and 40mm thickness in FRP molded grating 83*83H40 makes it suitable for industrial platforms, walkways, trench covers and flooring where load-bearing and slip resistance are required. Its open structure allows liquids and debris to pass through, and it is commonly used in corrosive environments such as chemical, water treatment, electroplating and marine engineering.
Selection Guidance
During selection, the resin system and grating thickness should be determined based on actual load, span, support method and service environment. The mesh and thickness parameters of 83*83H40 can be compared with other specifications in our molded grating series. Please contact us for detailed specifications and selection advice.
Product Advantages
FRP molded grating is molded from unsaturated polyester resin and fiberglass, offering characteristics such as light weight, high strength, corrosion resistance, slip resistance and insulation. The 83*83H40 mesh design balances load-bearing capacity and open area, making it easy to install and maintain.
Inquiry Guidance
If you need to know the resin type, color, surface treatment and packaging method of FRP molded grating 83*83H40, please contact us for detailed specifications and quotation. We can provide customized solutions according to your project requirements.
Operating Environment
- This molded FRP grating is built for both indoor and outdoor installations, such as walkways, platforms and stair treads in chemical plants, wastewater treatment facilities and offshore environments, where the unsaturated polyester resin matrix resists moisture and humidity.
- The isophthalic, vinyl ester and bisphenol-A type resins offer resistance to corrosive media including acids, alkalis and salts, making the grating suitable for areas with chemical splashes or fumes.
- With a flame-retardant formulation available (OFR-25, IFR-25, VEFR-25 and phenolic type), this grating is intended for applications where fire safety is a concern.
- For specific temperature ranges, chemical concentration limits and service conditions, please contact us for the full parameter list and application guidance.