FRP Molded Grating 50×50 H50 Light Duty


Contact us for a quotation

Product details

Genius FRP

 Glass fiber reinforced plastic ( FRP ) molding grid is a kind of plate material with a certain opening rate, which is made of unsaturated polyester resin ( including isophthalic up, linbenxing, type and fenquanxing, bisphenol ) as skeleton in the customization mold. 

Name

Content

Type

Resin

35%

OFR-25,IFR-25,VEFR-25

Fiberglass

33%

E

Filler

31%

ATH,PR

Others

1%

---

Introduction of raw materials

Resin type

Code

Resin type

Flame retardant property

Recommended usage occasions

MP-5

Phenolic type

Oxygen index can reach about 80

Low toxicity and high flame retardant, fire safety is very important for the occasion

VEFR-25

Vinyl type

Oxygen index 28 or above

Acid, alkali and other corrosive harsh environment

VEFR-10

Vinyl type

Oxygen index 35 or above

Flame retardant requirements of high acid, alkali and good occasions

IFR-25

Meta benzene

Oxygen index 28 or above

A VEFR type economy, and excellent, moderate acid alkali and solvent

IFGR-30

Benzene food grade

Oxygen index 26

Mainly used in meat products and food processing plants

OFR-25

Ortho type

Oxygen index 28 or above

General acid and alkali environment

OCR

Ortho type

Oxygen index below 28

OFR-25 economy, no flame retardant requirements

The type selection of coarse glass fiber  

Code

Coarse sand type

Recommended usage occasions

E

Non alkali sand

For high strength requirements and high corrosion resistance of the occasion

Selected filler type  

Code

Filler type

Recommended usage occasions

ATH

Aluminum hydroxide

Retardant, smoke suppression, corrosion-resistant occasions

PR

No filler, pure resin

For high corrosion-resistant applications

Groove type

Polished type

Shop sand type

50*50*50(mm)

Panel size available:

1800*4000,1524*4000,1220*3660,

1220*2440,915*3050 Bidirectional force.

Bearing bar thickness (Top/Bottom):7.0/5.0

Bearing bar center:50

Open Aera:78% 

Approx Weight:20.8kgs/m²

Liner load(units:mm)

Span in (mm)

Load in kn/m of widht (concentrated)

Maximum Recommended

Apparent E1*10^6 N-mm^2/m

4005.73011.8
60015.12114.9

Uniform load(units:mm)

Span in (mm)

Load in kn/sqm (uniformed)

Maximum Recommended

Apparent E1*10^6 N-mm^2/m

4001.415411.8
6005.77314.9
8001.63516.5

The characteristics:

  1. Corrosion Resistant 

  2. Slip Resistant 

  3. Superior Ergonomics 

  4. Low Install Cost 

  5. Fire Retardant 

  6. Lightweight,Bi-directional Strength, and the cutting makes the pipes easier to install.

  7. The internal and external uniform color and color can be arbitrary choice.

  8. It has good social and economic benefits.

  9. Can design , flexible and varied size, size stability

Widely used in:

Genius FRP grating is widely used in landing (industrial) floor, stairs and walkways and platforms. Using glass fiber reinforced plastic grille has many advantages: glass fiber reinforced plastic grille, weather resistance, low maintenance cost, has a long service life and good anti-skid performance. In addition, the glass fiber reinforced plastic grille is simple, fast, flexible processing and assembly.  


Application Scenarios

The FRP molded grating 50×50 H50 light duty type is suitable for walkways, operating platforms, trench covers, stair treads and light-load supporting applications in various corrosive environments. Its mesh structure and light-duty design facilitate cutting and installation, and it can be flexibly adjusted to on-site dimensions. Please contact us to confirm the specific operating conditions.

Selection Guidance

When selecting, please take into account load requirements, span, the corrosiveness and flame retardant requirements of the service environment, and the installation method. This product is a 50×50 mm mesh, 50 mm thick light-duty specification. If you need different load ratings, resin systems or colors, please contact us for detailed specifications and selection advice.

Product Advantages

Molded from unsaturated polyester resin and fiberglass, it features corrosion resistance, light weight and high strength, slip resistance and insulation, and maintenance-free operation. It is also water-permeable, light-transmitting and easy to process on site. Different resin systems vary in their emphasis on flame retardancy and chemical resistance, and can be selected as needed. For more performance details, please contact us.

Inquiry Guidance

For detailed specifications, resin options, color customization, packaging and delivery arrangements of this product, please contact us for a detailed quotation and technical support. Please provide your application scenario and quantity requirements, and we will recommend a suitable solution for you.