Greenlogy TEC

FRP molded grating is a panel with a certain open area, made with unsaturated polyester resin (including isophthalic, orthophthalic, phenolic and bisphenol types) as the framework and formed in custom molds.

Name

Content

Type

Resin

35%

OFR-25,IFR-25,VEFR-25

Glass fiber

33%

E

Filler

31%

ATH,PR

Others

1%

---

Introduction to raw materials

Resin type

Code

Resin type

Flame retardant performance

Recommended applications

MP-5

Phenolic type

Oxygen index up to approximately 80

Low toxicity, high flame retardancy; applications where fire safety is critical

VEFR-25

Vinyl ester type

Oxygen index 28 and above

Harsh corrosive environments such as acids and alkalis

VEFR-10

Vinyl ester type

Oxygen index 35 and above

Acid and alkali environments with high flame retardant requirements and applications requiring good performance

IFR-25

Isophthalic type

Oxygen index 28 and above

VEFR economical type, good performance, resistant to moderate acids, alkalis and solvents

IFGR-30

Food-grade resin

Oxygen index 26

Mainly used for meat products and food processing plants

OFR-25

Orthophthalic type

Oxygen index 28 and above

General acid and alkali environments

OCR

Orthophthalic type

Oxygen index below 28

OFR-25 economical type, no flame-retardant requirement

Selection of coarse glass fiber type  

Code

Coarse grit type

Recommended applications

E

Alkali-free (E-glass) grit

For high-strength requirements and highly corrosion-resistant applications

Selection of filler type  

Code

Filler type

Recommended applications

ATH

Aluminum hydroxide

Flame-retardant, smoke-suppressing and corrosion-resistant applications

PR

No filler, pure resin

For highly corrosion-resistant applications

Channel type

Polished type

Workshop sand type

50*50*50(mm)

Available panel dimensions:

1800*4000,1524*4000,1220*3660,

1220*2440,915*3050 Bi-directional load bearing.

Load-bearing flat bar thickness (top/bottom): 8.0/6.0

Load-bearing flat bar center spacing: 50

Open area: 78%

Approximate weight: 23.7 kgs/m²

Line load (unit: mm)

Deflection

kg/m

kg/m

kg/m

kg/m

kg/m

kg/m

Ultimate

Span (mm)

150

300

450

600

750

1500

Load

3000.310.410.480.641.041.4521727
6000.510.811.231.753.334.2711713
9001.122.243.25.166.5813.57780
12001.332.615.989.9511.9---5834

Uniformly distributed load (unit: mm)

Deflection

kg/m²

kg/m²

kg/m²

kg/m²

kg/m²

kg/m²

kg/m²

Span (mm)

240

480

980

1450

2450

3650

4880

3000.250.280.330.380.480.74---
6000.380.580.971.372.134.12---
9001.192.113.945.779.4518.6---
12002.414.939.961516.821.6---

Features:

  1. Corrosion resistant 

  2. Slip resistant 

  3. Ergonomic design 

  4. Low installation cost 

  5. Flame retardant 

  6. Lightweight with high bi-directional strength; cut pipes are easier to install.

  7. Uniform color inside and outside; colors can be selected freely.

  8. Delivers favorable social and economic benefits.

  9. Designable, flexible and diverse in size, dimensionally stable

Widely used in:

Greenlogy TEC FRP grating is widely used for industrial stair platforms, floors, stairs, walkways and platforms. Using FRP grating offers many advantages: good weather resistance, low maintenance cost, long service life and good anti-slip performance. In addition, FRP grating is simple, fast and flexible to process and assemble.


Application scenarios

Molded FRP grating is widely used for operating platforms, walkways, stair treads and trench covers in chemical, petroleum, power, wastewater treatment, marine engineering and other fields. Its corrosion resistance, anti-slip performance and high strength-to-weight ratio make it perform well in harsh environments such as damp and acid-alkali conditions.

Selection guide

Selection requires comprehensive consideration of load requirements, span, corrosive environment and fire rating. Different resin types (such as orthophthalic, isophthalic, vinyl ester and phenolic) suit different corrosive media and temperature conditions. Contact us for detailed specifications and selection advice; we will provide a suitable solution based on your operating conditions.

Product advantages

Molded FRP grating features excellent corrosion resistance, high strength-to-weight ratio, anti-slip performance, insulation and maintenance-free operation, with a long service life and simple installation. Compared with traditional metal grating, it can significantly reduce maintenance costs, especially in highly corrosive environments.

Inquiry guidance

For more product information, technical parameters or a quotation, please contact us. Please provide your specific application scenario, dimensional requirements and quantity, and we will provide professional support as soon as possible.

Operating environment

  • Molded FRP grating 50*50H50 can be used long-term outdoors in open-air applications such as platforms, walkways and trench covers; its unsaturated polyester resin system combined with E-glass fiber can withstand sun and rain as well as alternating temperature and humidity changes.
  • In chemical, electroplating, wastewater treatment and other locations where acid, alkali and salt corrosive media are present, grating with isophthalic, vinyl ester or phenolic resin can be selected according to the medium type to meet the corresponding corrosion resistance and flame retardant requirements.
  • In damp areas prone to water accumulation or requiring washing and cleaning, the open-cell structure of molded grating facilitates liquid drainage, making it suitable for use as operating platforms and floor paving material.
  • For indoor or semi-enclosed spaces with higher fire safety requirements, high flame-retardant resin models can be selected; please consult us to confirm the selection based on the temperature, medium concentration and flame retardant rating requirements of the specific operating environment.