Product Category

Product details

Genius FRP  

 Glass fiber reinforced plastic ( FRP ) molding grid is a kind of plate material with a certain opening rate, which is made of unsaturated polyester resin ( including isophthalic up, linbenxing, type and fenquanxing, bisphenol ) as skeleton in the customization mold. 

Name

Content

Type

Resin

35%

OFR-25,IFR-25,VEFR-25

Fiberglass

33%

E

Filler

31%

ATH,PR

Others

1%

---

Introduction of raw materials

Resin type

Code

Resin type

Flame retardant property

Recommended usage occasions

MP-5

Phenolic type

Oxygen index can reach about 80

Low toxicity and high flame retardant, fire safety is very important for the occasion

VEFR-25

Vinyl type

Oxygen index 28 or above

Acid, alkali and other corrosive harsh environment

VEFR-10

Vinyl type

Oxygen index 35 or above

Flame retardant requirements of high acid, alkali and good occasions

IFR-25

Meta benzene

Oxygen index 28 or above

A VEFR type economy, and excellent, moderate acid alkali and solvent

IFGR-30

Benzene food grade

Oxygen index 26

Mainly used in meat products and food processing plants

OFR-25

Ortho type

Oxygen index 28 or above

General acid and alkali environment

OCR

Ortho type

Oxygen index below 28

OFR-25 economy, no flame retardant requirements

The type selection of coarse glass fiber  

Code

Coarse sand type

Recommended usage occasions

E

Non alkali sand

For high strength requirements and high corrosion resistance of the occasion

Selected filler type  

Code

Filler type

Recommended usage occasions

ATH

Aluminum hydroxide

Retardant, smoke suppression, corrosion-resistant occasions

PR

No filler, pure resin

For high corrosion-resistant applications

Groove type

Polished type

Shop sand type

50*50*40(mm)

Panel size available:

1788*4531,1225*5035 Bidirectional force.

Bearing bar thickness (Top/Bottom):6.8/5.0

Bearing bar center:50

Open Aera:80%

Approx Weight:15.82kgs/m²

Liner load(units:mm)

Span in (mm)

Load in kn/m of widht (concentrated)

Maximum Recommended

Apparent E1*10^6 N-mm^2/m

4004.43011.8
60011.82114.9

Uniform load(units:mm)

Span in (mm)

Load in kn/sqm (uniformed)

Maximum Recommended

Apparent E1*10^6 N-mm^2/m

4001.115411.8
6004.47314.9
8001.33516.6

The characteristics:

  1. Corrosion Resistant 

  2. Slip Resistant 

  3. Superior Ergonomics 

  4. Low Install Cost 

  5. Fire Retardant 

  6. Lightweight,Bi-directional Strength, and the cutting makes the pipes easier to install.

  7. The internal and external uniform color and color can be arbitrary choice.

  8. It has good social and economic benefits.

  9. Can design , flexible and varied size, size stability

Widely used in:

Genius FRP grating is widely used in landing (industrial) floor, stairs and walkways and platforms. Using glass fiber reinforced plastic grille has many advantages: glass fiber reinforced plastic grille, weather resistance, low maintenance cost, has a long service life and good anti-skid performance. In addition, the glass fiber reinforced plastic grille is simple, fast, flexible processing and assembly.   


Application Scenarios

FRP molded grating 50*50 H40 is commonly used for working platforms, walkways, trench covers, stair treads and equipment operating surfaces that require slip resistance, corrosion resistance and load-bearing capacity. Its 50 mm mesh and 40 mm height suit applications needing open drainage, ventilation or reduced self-weight. For suitability under specific working conditions, please contact us to evaluate together with site conditions.

Selection Guide

During selection, first clarify load-bearing requirements, span, corrosive media and fire protection requirements, then determine the resin system, grating thickness and mesh size accordingly. Different resin types have different emphases in chemical resistance and flame retardant performance, and need to match the service environment. Please contact us for detailed specifications and selection advice.

Product Advantages

Molded grating is formed as a whole, with fibers and resin evenly distributed. It combines light weight, high strength, corrosion resistance and two-way load-bearing characteristics, with a slip-resistant surface that is easy to cut and install. Compared with traditional metal grating, it is more suitable for humid, acid-base or salt-spray environments. For specific performance details, please contact us for more information.

Inquiry Guide

To confirm whether FRP molded grating 50*50 H40 is suitable for your project, please provide the service environment, load-bearing requirements and size requirements, and we will help match a solution. Please contact us for detailed specifications and a quotation.

Operating Environment

  • This molded FRP grating (50×50 mm mesh, 40 mm depth) is built from unsaturated polyester resin, so it suits both indoor and outdoor installations where moisture and weather exposure are present.
  • The corrosion-resistant resin skeleton makes it suitable for service around the chemical, wastewater and process-plant areas where aggressive media would attack metal gratings.
  • With the phenolic-type resin option offering high flame-retardant performance and low toxicity, this grating can be used in areas where fire safety is a concern.
  • Its E-glass fiber reinforcement keeps the panel stable under humid and varying outdoor conditions; contact us for the full parameter list for your specific environment.