Product Category

Product details

Greenlogy TEC

FRP molded grating is a panel with a certain open area, made in custom molds with unsaturated polyester resin (including isophthalic, orthophthalic, phenolic and bisphenol types) as the matrix.

Name

Content

Type

Resin

35%

OFR-25,IFR-25,VEFR-25

Glass fiber

33%

E

Filler

31%

ATH,PR

Other

1%

---

Raw material introduction

Resin type

Code

Resin type

Flame retardancy

Recommended applications

MP-5

Phenolic type

Oxygen index up to about 80

Low toxicity, high flame retardancy; suitable for applications with very high fire safety requirements

VEFR-25

Vinyl ester type

Oxygen index 28 and above

Harsh corrosive environments such as acids and alkalis

VEFR-10

Vinyl ester type

Oxygen index above 35

High acid and alkali environments with flame retardancy requirements and good performance applications

IFR-25

Isophthalic type

Oxygen index 28 and above

VEFR economical type, good performance, resistant to moderate acids, alkalis and solvents

IFGR-30

Benzene-based, food grade

Oxygen index 26

Mainly used in meat processing and food processing plants

OFR-25

Orthophthalic type

Oxygen index 28 and above

General acid and alkali environments

OCR

Orthophthalic type

Oxygen index below 28

OFR-25 economical type, no flame retardancy requirement

Selection of coarse glass fiber  

Code

Coarse grit type

Recommended applications

E

E-glass grit

For applications requiring high strength and high corrosion resistance

Selection of filler type 

Code

Filler type

Recommended applications

ATH

Aluminum hydroxide

Flame-retardant, smoke-suppressing and corrosion-resistant applications

PR

No filler, pure resin

For high corrosion resistance applications

Grooved type

Polished type

Sand-cast molded workshop surface

50*50*25(mm)

Available panel sizes:

1220*3660,1220*2440,915*3050 

Bidirectional load bearing.

Load-bearing flat bar thickness (top/bottom): 7.5/6.0

Load-bearing flat bar center spacing: 50

Open area: 78%

Approx. weight: 11.5 kgs/m²

Line load (unit: mm)

Span (mm)

Load per meter width (kN/m, concentrated load)

Maximum recommended value

Apparent E1*10^6 N-mm^2/m

4002.83011.8
6007.62114.9

Uniformly distributed load (unit: mm)

Span (mm)

Load (kN/sqm, uniformly distributed)

Maximum recommended value

Apparent E1*10^6 N-mm^2/m

4000.715411.8
6002.87314.9
8000.83516.5

Features:

  1. Corrosion resistant

  2. Slip resistant

  3. Superior ergonomic design

  4. Low installation cost

  5. Flame retardant

  6. Lightweight with high bidirectional strength; cutting makes the grating easier to install.

  7. Uniform interior and exterior color, with colors freely selectable.

  8. Delivers favorable social and economic benefits.

  9. Can be designed, with flexible and diverse sizes and stable dimensions

Widely used in:

Greenlogy TEC FRP grating is widely used for platform (industrial) flooring, stairways, walkways and platforms. Using fiberglass reinforced plastic grating offers many advantages: FRP grating has good weather resistance, low maintenance cost, long service life and good anti-slip performance. In addition, FRP grating is simple, fast and flexible to process and assemble.


Application Scenarios

FRP molded grating 50*50H25 is commonly used for operating platforms, walkways and trench covers in corrosive environments such as chemical, electroplating and wastewater treatment, and is also suitable for marine engineering, ship decks and other applications requiring salt-spray resistance. Its 25 mm thickness balances load-bearing capacity and light weight, making it suitable for medium- and low-load pedestrian walkways or equipment supports. For selection advice for specific working conditions, please contact us.

Selection Guide

Selection should comprehensively consider the resin type (such as orthophthalic, isophthalic, vinyl ester, etc.), grating thickness, mesh size, load requirements and operating environment. Different resins emphasize different properties such as corrosion resistance and flame retardancy; for example, isophthalic resin has better water resistance, while vinyl ester resin resists strong corrosion. We recommend that you provide specific application conditions, and our technical team will assist you in choosing the right product.

Product Advantages

FRP molded grating features light weight and high strength, corrosion resistance, anti-slip, insulation and maintenance-free performance, with a long service life and convenient installation. Its mesh structure allows fluids to pass through, reducing water accumulation and debris buildup. Compared with metal grating, FRP grating is more durable in wet and corrosive environments and requires no regular painting.

Inquiry Guidance

For detailed specifications, prices and supply information on FRP molded grating 50*50H25, please contact us for professional consultation and a quotation. We can provide customized solutions according to your needs.

Operating Environment

  • The 50×50 mm mesh, 25 mm thick FRP molded grating is designed for indoor and outdoor use in industrial facilities, including weather-exposed walkways, platforms and stair treads.
  • The isophthalic, vinyl ester and bisphenol A unsaturated polyester resin systemsmolded FRP grating can withstand the humid, wet and chemically corrosive atmospheres encountered in processing plants, water treatment and chemical handling areas.
  • Its corrosion-resistant fiberglass reinforced plastic construction is suitable for locations where weak acids, weak alkalis or salts may be present, helping to extend service life compared with conventional materials.
  • For detailed temperature limits, chemical resistance tables or load tables, please contact us to request the full technical data sheet.