FRP Molded Grating 38*38H30 (OFR-25)


Contact us for a quotation

Product details

Greenlogy TEC  

FRP molded grating is a panel with a certain open area, made with unsaturated polyester resin (including isophthalic, orthophthalic, phenolic and bisphenol types) as the matrix and produced in custom molds.

Name

Content

Type

Resin

35%

OFR-25,IFR-25,VEFR-25

Glass fiber

33%

E

Filler

31%

ATH,PR

Others

1%

---

Introduction to raw materials

Resin type

Code

Resin type

Flame retardant performance

Standard color

Recommended applications

MP-5

Phenolic type

Oxygen index up to about 80

Brown

Low toxicity and high flame retardancy; applications with high fire safety requirements

VEFR-25

Vinyl type

Oxygen index above 28

Grass green, yellow, gray, orange

Harsh corrosive environments such as acids and alkalis

VEFR-10

Vinyl type

Oxygen index above 35

Dark gray, black

For applications requiring high acid and high alkali resistance and good flame retardancy

IFR-25

Isophthalic type

Oxygen index above 28

Grass green, yellow, gray

VEFR type is economical with good performance, resistant to moderate acids, alkalis and solvents

IFGR-30

Phthalic anhydride type, food grade

Limiting oxygen index 26

Yellow

Mainly used in meat processing and food processing plants

OFR-25

Orthophthalic type

Oxygen index above 28

Grass green, yellow, gray

General acid and alkali environments

OCR

Orthophthalic type

Limiting oxygen index below 28

Green, yellow, gray

OFR-25 economical type, no flame retardancy requirement

Coarse fiberglass type selection 

CodeCoarse fiber typeRecommended applications

E

Alkali-free (E-glass) fiber

For applications requiring high strength and high corrosion resistance

Selected filler type 

Code

Filler type

Recommended applications

ATH

Aluminum hydroxide

Flame-retardant, smoke-suppressing and corrosion-resistant applications

PR

Unfilled, pure resin

Suitable for high-corrosion-resistance applications

Grooved type

Polished type

Workshop sanded finish

38*38*30(mm)

Optional panel sizes:

1524*4000,1220*4000,1220*3660,1220*2440,915*3050 Bidirectional load bearing.     

Load-bearing flat bar thickness (top/bottom): 6.0/5.0

Load-bearing flat bar center spacing: 38

Open area: 68%

Approximate weight: 14.6 kgs/m²

Line load (unit: mm)

Deflection

kg/m

kg/m

kg/m

kg/m

kg/m

kg/m

Ultimate 

Span (mm)

751503004507501500

Load

300<0.25<0.250.250.510.761.529923.4
4500.250.511.021.522.543.924827.6
6000.511.272.293.565.847.384112.4
7501.272.544.837.3712.516.03173.7
9002.274.549.0813.618.722.12637.3

Uniformly distributed load (unit: mm)

Deflection

kg/m²

kg/m²

kg/m²

kg/m²

kg/m²

kg/m²

Span (mm)

350500750100015002500
3000.290.480.570.751.151.82
4500.781.191.812.473.544.95
6001.762.664.285.568.4113.2
7503.485.128.2111.016.42---
9005.898.8114.218.9------

Features:

  1. Corrosion-resistant 

  2. Slip-resistant 

  3. Excellent ergonomic design 

  4. Low installation cost 

  5. Flame-retardant 

  6. Lightweight with high bidirectional strength; cutting makes the panels easier to install.

  7. Uniform color inside and out; colors can be selected freely.

  8. Delivers favorable social and economic benefits.

  9. Flexible design, a variety of sizes, and dimensional stability

 

Widely used in:

Greenlogy TEC FRP grating is widely used for platform (industrial) flooring, stairways, walkways and platforms. Using FRP grating offers many advantages: good weather resistance, low maintenance cost, long service life and good slip resistance. In addition, FRP grating is simple, fast and flexible to fabricate and assemble.


Application scenarios

FRP molded grating 38*38H30 is suitable for corrosive environments such as chemical plants, wastewater treatment and marine engineering, and can also be used as platforms, walkways, trench covers and other applications requiring slip resistance and corrosion resistance. Its lightweight, high-strength characteristics make it an ideal alternative to conventional metal grating.

Selection guidance

When selecting, consider the resin type (such as orthophthalic, isophthalic and vinyl ester types) to suit different corrosion resistance requirements, and choose the appropriate grating thickness and mesh size according to load requirements. For detailed technical parameters and selection advice, please contact us for professional guidance.

Product advantages

This grating features excellent corrosion resistance, light weight and high strength, slip resistance, insulation and easy installation, along with low maintenance cost and long service life. The molded process ensures dimensional stability and a smooth surface, and colors can be customized on request.

Inquiry guidance

For specific specifications, pricing or customization requirements for FRP molded grating 38*38H30, please contact us via the contact details on this website, and we will provide a detailed quotation and technical support.

Service environment

  • This FRP molded grating is molded from unsaturated polyester resin (including orthophthalic, bisphenol and phenolic types) combined with glass fiber, and can be used for indoor and outdoor installation.
  • Molded mesh structures with a specific open area are typically used in industrial plants and process areas where corrosive media, moisture and humid atmospheres are present.
  • For installations exposed to specific chemicals, temperature or humidity conditions, please select a resin type that matches the actual service environment (for example, phenolic type may be chosen where low toxicity and high flame retardancy are required).
  • Please contact us for the complete parameter table and to confirm the resin grade and glass fiber content suitable for your operating conditions.