Product Category

Product details

Greenlogy TEC

FRP molded grating is a panel with a certain open area, made with unsaturated polyester resin (including isophthalic, orthophthalic, phenolic and bisphenol types) as the framework and produced in custom molds.

Name

Content

Type

Resin

35%

OFR-25,IFR-25,VEFR-25

Glass fiber

33%

E

Filler

31%

ATH,PR

Others

1%

---

 Raw material introduction

Resin type

Code

Resin type

Flame retardant performance

Recommended applications

MP-5

Phenolic type

Oxygen index up to about 80

Low toxicity and high flame retardancy, for applications with very high fire safety requirements

VEFR-25

Vinyl ester type

Oxygen index 28 and above

Harsh corrosive environments such as acids and alkalis

VEFR-10

Vinyl ester type

Oxygen index above 35

Strong acids and strong alkalis with high flame retardant requirements and applications requiring good performance

IFR-25

Isophthalic type

Oxygen index 28 and above

VEFR economical type, good performance, resistant to moderate acids, alkalis and solvents

IFGR-30

Benzene-type, food grade

Oxygen index 26

Mainly used in meat processing and food processing plants

OFR-25

Orthophthalic type

Oxygen index 28 and above

General acid and alkali environments

OCR

Orthophthalic type

Oxygen index below 28

OFR-25 economical type, no flame retardancy requirement

  Coarse glass fiber selection   

Code

Coarse grit type

Recommended applications

E

E-glass grit

For applications requiring high strength and high corrosion resistance

Filler type selection  

Code

Filler type

Recommended applications

ATH

Aluminum hydroxide

Flame-retardant, smoke-suppressing and corrosion-resistant applications

PR

No filler, pure resin

For high corrosion resistance applications

Grooved type

Polished type

Workshop sand-surface type

38*38*30(mm)

Available panel sizes:

1220*4000,1220*3660,1220*2440,

915*3050 Bidirectional load bearing.     

Load-bearing flat bar thickness (top/bottom): 6.0/5.0

Load-bearing flat bar center distance: 38

Open area: 78%

Approximate weight: 6.00 kgs/m²

Linear load (unit: mm)

Span (mm)

Load, unit kN/m width (concentrated)

Maximum

Recommended

Apparent E1*10^6 N-mm^2/m

40024197.14
6006.8138.55
80015.4109.02

Uniform load (unit: mm)

Span (mm)

Load, unit kN/m² (uniform)

Maximum

Recommended

Apparent E1*10^6 N-mm^2/m

4000.61007.14
6002.6458.55
8007.7269.02

Features:

  1. Corrosion resistant 

  2. Slip resistant 

  3. Superior ergonomic design 

  4. Low installation cost 

  5. Flame retardant 

  6. Lightweight with high bidirectional strength; cutting makes piping easier to install.

  7. Uniform color inside and out; colors can be selected freely.

  8. Delivers good social and economic benefits.

  9. Designable, flexible and diverse in size, and dimensionally stable

Widely used in:

Greenlogy TEC FRP grating is widely used for platform (industrial) flooring, stairways, walkways and platforms. Using FRP grating offers many advantages: good weather resistance, low maintenance cost, long service life and good anti-slip performance. In addition, FRP grating is simple, fast and flexible to process and assemble.


Application scenarios

FRP molded grating 38*38H13 uses a 38 mm × 38 mm mesh with a 13 mm thick structure, suitable for platform walkways, trench covers, stair treads and various industrial and civil applications requiring anti-slip, corrosion resistance and water permeability. For specific solutions under different media and load environments, please contact us to evaluate against your operating conditions.

Selection guide

Selection should comprehensively consider resin type (such as orthophthalic, isophthalic, vinyl ester, phenolic, etc.), load requirements, corrosive media and installation method. The 38*38H13 specification has defined mesh size and thickness, making it easy to fit with other structural components. To determine the most suitable resin system and panel type, please contact us for detailed specifications and selection advice.

Product advantages

Molded grating uses unsaturated polyester resin as the matrix and glass fiber as reinforcement, molded in a single operation. It features light weight, high strength, corrosion resistance, anti-slip performance and easy cutting and installation; the 38*38H13 mesh and thickness combination balances water permeability and load performance. Specific performance advantages can be further explained based on your operating environment; please contact us to discuss.

Inquiry guide

To learn about the detailed specifications, resin options, colors, packaging and delivery methods of FRP molded grating 38*38H13, please contact us for detailed specifications and a quotation. We will provide a targeted solution based on your project requirements.