Product Category

Product details

Genius FRP     

Glass fiber reinforced plastic ( FRP ) molding grid is a kind of plate material with a certain opening rate, which is made of unsaturated polyester resin ( including isophthalic up, linbenxing, type and fenquanxing, bisphenol ) as skeleton in the customization mold. 

Name

Content

Type

Resin

35%

OFR-25、IFR-25、VEFR-25

Fiberglass

33%

E

Filler

31%

ATH、PR

Others

1%

---

Introduction of raw materials

 Resin type  

Code

Resin type

Flame retardant property

Recommended usage occasions

MP-5

Phenolic type

Oxygen index can reach about 80

Low toxicity and high flame retardant, fire safety is very important for the occasion

VEFR-25

Vinyl type

Oxygen index 28 or above

Acid, alkali and other corrosive harsh environment

VEFR-10

Vinyl type

Oxygen index 35 or above

Flame retardant requirements of high acid, alkali and good occasions

IFR-25

Meta benzene

Oxygen index 28 or above

A VEFR type economy, and excellent, moderate acid alkali and solvent

IFGR-30

Benzene food grade

Oxygen index 26

Mainly used in meat products and food processing plants

OFR-25

Ortho type

Oxygen index 28 or above

General acid and alkali environment

OCR

Ortho type

Oxygen index below 28

OFR-25 economy, no flame retardant requirements

The type selection of coarse glass fiber  

Code

Coarse sand type

Recommended usage occasions

E

Non alkali sand

For high strength requirements and high corrosion resistance of the occasio

Selected filler type  

Code

Filler type

Recommended usage occasions

ATH

Aluminum hydroxide

Retardant, smoke suppression, corrosion-resistant occasions

PR

No filler, pure resin

For high corrosion-resistant applications

Groove type

Polished type

Shop sand type

25*100*38(mm)

Panel size available:

1220*3660 Width stress 

Bearing bar thickness (Top/Bottom):8.0/6.0

Bearing bar center:25

Open Aera:62%

Approx Weight:22.5kgs/m²

The characteristics:

  1. Corrosion Resistant 

  2. Slip Resistant 

  3. Superior Ergonomics 

  4. Low Install Cost 

  5. Fire Retardant 

  6. Lightweight,Bi-directional Strength, and the cutting makes the pipes easier to install.

  7. The internal and external uniform color and color can be arbitrary choice.

  8. It has good social and economic benefits.

  9. Can design , flexible and varied size, size stability

Widely used in:

Genius FRP grating is widely used in landing (industrial) floor, stairs and walkways and platforms. Using glass fiber reinforced plastic grille has many advantages: glass fiber reinforced plastic grille, weather resistance, low maintenance cost, has a long service life and good anti-skid performance. In addition, the glass fiber reinforced plastic grille is simple, fast, flexible processing and assembly.  





Application Scenarios

FRP molded grating 25*100H38 is suitable for walkways, platforms, trench covers, stair treads and equipment operating surfaces that require slip resistance, corrosion resistance and load-bearing capacity. It is commonly used in humid or corrosive environments such as chemical, water treatment, power and marine engineering. Because molded grating is integrally molded with an open mesh structure, it is also suitable for applications requiring drainage, light transmission or reduced self-weight. For specific environment suitability, please contact us for detailed specifications and quotations.

Selection Guidance

During selection, the resin type, grating thickness and mesh size should be determined comprehensively based on actual loads, support spans, corrosive media and temperature of the service environment, and whether flame retardancy or insulation is required. Under the same 25*100H38 specification, different resin formulations perform differently in chemical resistance and flame retardancy. We recommend providing your working conditions so we can assist in recommending a suitable configuration. Please contact us for detailed specifications and quotations.

Product Advantages

Molded grating is integrally molded from resin and fiberglass, featuring light weight, high strength, corrosion resistance, slip resistance, insulation and maintenance-free characteristics. Compared with traditional metal grating, it has a longer service life in corrosive environments. The mesh structure facilitates cutting and on-site installation, and different resin systems can be selected as needed to balance chemical resistance and flame retardant performance. For specific performance, please contact us for detailed specifications and quotations.

Inquiry Guidance

To confirm the available resin types, colors, surface treatments and supply solutions for 25*100H38 molded grating, please contact us and provide your service environment and dimensional requirements so we can assist with selection. Bulk purchases, customized specifications and requests for technical documents are all welcome for direct discussion. Please contact us for detailed specifications and quotations.